Structure Feature: | Ring Form Filler |
---|---|
Acid Resistance: | >99.6% |
Alkali Resistance: | >85% |
Still deciding? Get samples of US$ 0/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
ceramic cross partition ring has excellent acid resistance and heat resistance. It can resist to corrosion of various inorganic acids, organic acids and organic solvents except hydrofluoric acid, and can be used in high or low temperature conditions. Consequently the application range is very wide. The packing can be used in the drying columns, absorbing columns, cooling towers, scrubbing towers and actifier columns in chemical industry, metallurgy industry, coal gas industry, oxygen producing industry, etc.
Chemical Composition
Composition |
Value |
SiO2 |
>73% |
Al2O3 |
17-25% |
Fe2O3 |
<1.0% |
CaO |
<0.5% |
MgO |
<0.5% |
K2O+Na2O |
2-4% |
Other |
<0.1% |
Technical Parameter
Size |
Thickness |
Surface area |
Void Section |
Number |
Bulk Density |
80 |
8 |
120 |
54 |
1950 |
916 |
100 |
10 |
110 |
53 |
1000 |
930 |
150 |
15 |
60 |
58 |
296 |
960 |